Dumbass
Dumbass
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 91
Hi guys and girls
I am looking at building some light weight doors for a race truck and was wanting some advice on the layup. I will be infusing the parts, making an inner and outer skin and would like a carbon outer finish..
The catch is it is, they are for an off road vehicle and likely to fall on its side and hit trees and such (don't panic it has a roll cage) so kevlar will also be important to keep the boys safe from the carbon. and I will not be needing the window frame
I am not concerned about the life of the door against the trees but would like to have them able to open and close regularly without falling apart.
And is reusable silicon bagging worth looking at for the more complicated inside skin?
So any ideas would be greatly appreciated.
here is the truck
" alt="http://
">
Edited
12 Years Ago by
Dumbass
Reply
Like
3
Replies
andygtt
andygtt
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 157,
Visits: 1.2K
See the projects section for cars etc, I made carbon doors for my noble and heavily reinforced them with Kevlar to stop them falling apart in an 'accident'.
The simple fact is whilst the Kevlar will stop them falling to peices at the first tree you hit (as a full carbon one would), they will never be as robust as your steel doors...
Usually after an 'incident' a composite part will need replacing.
Reply
Like
2
Dumbass
Dumbass
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 91
Cheers for that, I shall have a nosey at your lay up
Yeah I understand that they will be a throw away item,
But I am still keen to do them due to the steel ones being difficult to open and painful when they close on you on big leans while getting out for winching..
So my main question is, Is a reusable silicon bag worth while? for the more complex inside skin.... The outer should be easy.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
I want to make some doors.
Dumbass
-
12 Years Ago
See the projects section for cars etc, I made carbon doors for my noble and heavily reinforced them...
andygtt
-
12 Years Ago
Cheers for that, I shall have a nosey at your lay up Yeah I understand that they will be a throw...
Dumbass
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search