Which is stronger for bending: tube or rod?


Author
Message
singcomposite
singcomposite
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Forum Members
Posts: 7, Visits: 10
mattias

I suggest you use customized tube with optimized layup angles. These available standard sized tubes may not meet your requirement.  
wozza
wozza
Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)Supreme Being (7.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
If you strengthen the wings it will probably break somewhere else. The wings may have been designed to be the weak point in order to protect the fuselage? 

Warren

Carbon Copies Ltd
Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It all depends on your circumstances.  6mm of solid rod will always be stiffer than 6mm OD tube.  However its a compromise between weight and strength, hence why tubes are often used.  In bending there is still tension and compression on the opposite sides of the tube/rod with less force in the middle, hence why with a reasonable wall thickness, the weight reduction more than offsets the slight strength loss from having a tube over a rod.

If you are stuck with 6mm, then a rod is your only option but with the added weight penalty. if not, id try a 8mm OD tube and see how you get on.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
mattias
mattias
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 1, Visits: 2
Hi,

I crashed my RC airplane (again!) and broke the 6x4mm carbon fiber tube in the wings.
I'm looking at replacing it with something stronger this time. The stresses are bending only - no tension or compression length-wise.

Which of the following would be the best?

  • 6mm carbon rod,
  • 6mm (4mm inner diameter) carbon tube,
  • 6x4mm carbon tube with a 4mm rod inside?


Thanks,

Mattias
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search