Which is stronger for bending: tube or rod?
Which is stronger for bending: tube or rod?
Post Reply
Like
6
Which is stronger for bending: tube or rod?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
mattias
mattias
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 2
Hi,
I crashed my RC airplane (again!) and broke the 6x4mm carbon fiber tube in the wings.
I'm looking at replacing it with something stronger this time. The stresses are bending only - no tension or compression length-wise.
Which of the following would be the best?
6mm carbon rod,
6mm (4mm inner diameter) carbon tube,
6x4mm carbon tube with a 4mm rod inside?
Thanks,
Mattias
Reply
Like
6
Reply
singcomposite
singcomposite
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 10
mattias
I suggest you use customized tube with optimized layup angles. These available standard sized tubes may not meet your requirement.
Tags
carbon fiber tubes
SingComposite
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Which is stronger for bending: tube or rod?
mattias
-
13 Years Ago
It all depends on your circumstances. 6mm of solid rod will always be stiffer than 6mm OD tube....
Warren (Staff)
-
13 Years Ago
If you strengthen the wings it will probably break somewhere else. The wings may have been designed...
wozza
-
13 Years Ago
mattias I suggest you use customized tube with optimized layup angles. These available standard...
singcomposite
-
12 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search