 Do any of you clever composite fellows have any ideas on creating a clean break line between a carbon skinned surface and a plain (painted) surface? I attempted masking with tape an area I did not want skinned but came to the quick realization that the resin would slightly cover the tape and not allow me to remove it. BAD PLAN !!!  
   All I know to do is to cure my carbon area, blend the nasty edge the best I can then repaint the area next to it. 
   Also would like do a motorcycle windscreen the same way (glass upper and carbon lower) but getting that break line attractive is not currently workable. 


Please advise,
     GEARHEAD
Replies
japcarmaniac
japcarmaniac
Supreme Being (539 reputation)Supreme Being (539 reputation)Supreme Being (539 reputation)Supreme Being (539 reputation)Supreme Being (539 reputation)Supreme Being (539 reputation)Supreme Being (539 reputation)Supreme Being (539 reputation)Supreme Being (539 reputation)
Group: Forum Members
Posts: 53, Visits: 157
can a coat of high temp epoxy be used all over instead of laquer?


Paul (Staff)
Paul (Staff)
Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)Technical Support (1.8K reputation)
Group: Administrators
Posts: 134, Visits: 614
Yes you can use a high temp black paint to blend the edges, just feather the paint in from the edge, I see no problem in then coating this with the high temp resin and then flatting it out and polishing it to a final finish. I could be wrong but I'm pretty sure you can get high temperature clear-coat paints that you could also use for the last 'gloss' coat.

Paul Statham
Easy Composites / Carbon Mods - Technical
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search