Any tips for achieving a "clean" break line while carbon skinning?


Any tips for achieving a "clean" break line while carbon skinning?
Author
Message
GEARHEAD
GEARHEAD
Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)Supreme Being (84 reputation)
Group: Forum Members
Posts: 6, Visits: 62
 Do any of you clever composite fellows have any ideas on creating a clean break line between a carbon skinned surface and a plain (painted) surface? I attempted masking with tape an area I did not want skinned but came to the quick realization that the resin would slightly cover the tape and not allow me to remove it. BAD PLAN !!!  
   All I know to do is to cure my carbon area, blend the nasty edge the best I can then repaint the area next to it. 
   Also would like do a motorcycle windscreen the same way (glass upper and carbon lower) but getting that break line attractive is not currently workable. 


Please advise,
     GEARHEAD