Hello everybody!

I have a question for you experts. I would like to know if do I have to take into consideration some special points before vacuum bagging a sandwich laminate with PU foam. Do I have to make holes in the foam necessarily? I'm afraid the air don't go up from the first skin and have bubbles on my laminate. Of course, I would paint the mould before with clear epoxy resin.

Is it a good idea to use Soric for vacuum bagging? as it is designed for infusion or RTM.....Thanks and have a nice and productive weekend!
Reply
chemie29
chemie29
Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)Supreme Being (124 reputation)
Group: Forum Members
Posts: 18, Visits: 75
Thanks for your answers. My question is if it is really necessary to use time consuming techniques? I mean, can I vacuum bag a laminate like this at a time?  [epoxy resin as "gel coat" + wet carbon fibre with epoxy resin + PU foam 4 mm + wet carbon fibre with epoxy resin]. I'm afraid thet the air don't "travel" across de foam core, or may be iti is not strictly necessary if first plies are well wetted...Thanks!