First project.


Author
Message
carbonlynx
carbonlynx
Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)Forum Guru (59 reputation)
Group: Forum Members
Posts: 3, Visits: 39
so i located a simple piece to make out of CF it was the gas tank tube cover. Hand lay up with vacuum to remove excess resin. the part didn't have to be pretty cause it would get covered anyways just wanted to try. not sure as to its specs other than it was three layers.



"I was put on this Earth to accomplish a many number of things. Right now i am so far behind i will never die." ~unkown
Tags
Reply
BoostSamurai
BoostSamurai
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 34, Visits: 413
Looks like it came out pretty well for a first attempt.  Good work!

JZX World Forums
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search