By carbonlynx - 5/8/2013 12:22:01 AM
so i located a simple piece to make out of CF it was the gas tank tube cover. Hand lay up with vacuum to remove excess resin. the part didn't have to be pretty cause it would get covered anyways just wanted to try. not sure as to its specs other than it was three layers.
|
By BoostSamurai - 7/7/2013 1:03:07 PM
Looks like it came out pretty well for a first attempt. Good work!
|
|