carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
I don't normally photograph an entire project, but seeing as I had some free sample prepregs from 2 different suppliers I thought I'd turn it into a giggle. They both know I use VTF, and they assured me that their materials would compete. They told me that although the materials are made for autoclave, that I should see promising results OOA. I didnt get my hopes up as Ive tried several before and they all sucked.

I thought I'd turn it into a simple little project to play with these samples. The idea was to take a wooden part (as wood is something I haven't replicated before) that had a simple shape (I didn't have much hope for snything that isnt VTF). Nothing that would take longer than a week. So here it is, from original part to polished carbon copy:

Original wood part:



I tryed using teak oil to seal it, but that didnt work, it just kept sucking the oil, grain was still open.



So I used aluminium tape:


Flanges:



I knew I was gonna have to sand the stripes left by the aluminium tape, so i took the safest route which was to take a mould off the B side, this would in turn become a plug which I could sand down, most likely sanding the gelcoat quite thin. If I sand too far into the gelcoat, I dont have to worry as I will be taking a proper mould off it later. So making of the plug, followed by the mould:












Sanded the lines down with a block, and tried to get rid of negatives on the flanges. You can see why I did it this way, the grey spot there is where I sanded through the gelcoat into the skin coat, theres other spots like it and you can start to see the grey show through the green:






Postcure:


Taking the ali off was a right bitch, and it left a residue which was even harder to take off. Next time, Ill find a better way to do this:


To the prepreg room! Sealed and released:


Thawing and cutting the material:



Layup:



Bagging:







Bake:


Fresh out the oven:



Releasing was this easy:



Oh dear, it seems there was a bit of bridging. Im not surprised. As Iv'e said before, nothing beats VTF. These two photos were sent straight to the sales rep. Hes sending another sample Blink:



No carbon is scarp though, so I battled on. My plan was to fill the voids, mask them and put black stripes at the ends:






Sanding:


Some peeps on here get paranoid about fillinf the pinholes and voids with dust. Its nothing to worry about, the dust is transparent, and a layer of clear will make it dissapear:



Before the next coat, I'll try something new, branding. I've got a vinyl cutter, plus I made all of my branding myself, so I have the vector files, seemed rude not to do it:





The masking didnt really work, but I think it looks quite cool, even if by accident:


So, more sanding and lacquering, until the pinholes were filled, now go up the grades 400, 600, 800, 1200, 1500, 3000 then compounds coarse then fine:





Finished product on my desk:


Determined not to be beat, I remembered the second sample I had. Along with some new found knowledge gained from this paper:

http://digitool.library.mcgill.ca/webclient/StreamGate?folder_id=0&dvs=1371902526959~725

You could read the whole thing, or I could summarize it to this:
DONT USE BREATHER!













As simple as it is, I did learn something.  If youre making a part out of wood, don't use ali tape. Two reasons.  First, You have to sand back the gelcoat to get the lines off, and hence making your mould weaker (unless you did the plug-mould method I did. And second, if the original is not sacrificial, youre going to have a hard time taking the ali and its adhesive off very carefully. WD40 got it off without staining it, but I wouldnt place a bet if it was a different wood that was untreated.

I will also be commencing production without breather on the part, just on the mould.

Overall good experience, and the tea tray sold for £150 (for a weeks work!). Hopefully you guys can take something from it too.


http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Edited 12 Years Ago by carboncactus
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
carboncactus (22/06/2013)
TomDesign (22/06/2013)
Also cactus i dont need to put extra fiberglass layers or something parts to be light and strong. i can easyli put 1 layer of pre preg 200gr and be good? what you think for car fenders?


I never put fibreglass in anything I do unless the customer requests it to save money. It adds weight and its dishonest. A lot of people out there are putting only 1 layer of carbon and backing up with glass. It gets on my nerves.

Those trays were 4 layers of 200g carbon each.
The bike mudguard was one of 200g, one of 600g


Also as bad in my opinion is simply taking a mould off someones hard work and then reproducing it (often badly) and selling it as there own because they lack the skills to design and manufacture a part from scratch.
I have been involved in Composites for over 25 years and have had lots of my work copied some of which even have Patents.
As for CSM, E-Glass, Soric, Closed Cell Foam and other Core Materials they all have a major part to play in Advanced Composites. Used correctly and with honesty they can actually add and increase the performance of a part. I for one would not want to fit an "all carbon" bonnet to the front of a road car. If the worst happens and a pedestrian is hit then they will be pierced with shards of Carbon Fibre.
For me there is a massive difference between "Bling" and Composites.
Some  people may now see the deliberate irony in my chosen company name Wink

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
wozza - 12 Years Ago
TomDesign - 12 Years Ago
TomDesign - 12 Years Ago
Greg - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
CarbonMike - 12 Years Ago
morepower - 12 Years Ago
carboncactus - 12 Years Ago
morepower - 12 Years Ago
Warren (Staff) - 12 Years Ago
TomDesign - 12 Years Ago
morepower - 12 Years Ago
TomDesign - 12 Years Ago
morepower - 12 Years Ago
TomDesign - 12 Years Ago
morepower - 12 Years Ago
TomDesign - 12 Years Ago
morepower - 12 Years Ago
wozza - 12 Years Ago
morepower - 12 Years Ago
wozza - 12 Years Ago
carboncactus - 12 Years Ago
wozza - 12 Years Ago
morepower - 12 Years Ago
carboncactus - 12 Years Ago
morepower - 12 Years Ago
carboncactus - 12 Years Ago
morepower - 12 Years Ago
wozza - 12 Years Ago
TomDesign - 12 Years Ago
wozza - 12 Years Ago
fgayford - 12 Years Ago
Warren (Staff) - 12 Years Ago
TomDesign - 12 Years Ago
TomDesign - 12 Years Ago
morepower - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
             yes
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
     in lithuania
TomDesign - 12 Years Ago
morepower - 12 Years Ago
TomDesign - 12 Years Ago
morepower - 12 Years Ago
Greg - 12 Years Ago
morepower - 12 Years Ago
carboncactus - 12 Years Ago
Greg - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
morepower - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
carboncactus - 12 Years Ago
TomDesign - 12 Years Ago
TomDesign - 12 Years Ago
morepower - 12 Years Ago
TomDesign - 12 Years Ago
FiftyPence - 12 Years Ago
Tominator - 12 Years Ago
carboncactus - 12 Years Ago
Tominator - 12 Years Ago
carboncactus - 12 Years Ago
andygtt - 12 Years Ago
Warren (Staff) - 12 Years Ago
matthieutje65 - 12 Years Ago
morepower - 12 Years Ago
andygtt - 12 Years Ago
andygtt - 12 Years Ago
carboncactus - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search