Is it worthwhile degassing my coating resin in my vacuum chamber?
Is it worthwhile degassing my coating resin in my vacuum chamber?
Post Reply
Like
3
Is it worthwhile degassing my coating resin in my vacuum chamber?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
FiftyPence
FiftyPence
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 26,
Visits: 264
Is it worthwhile degassing my coating resin in my easycomposites vacuum chamber before brushing it onto my part?
Thanks in advance for your advice.
Reply
Like
3
Replies
benet
benet
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 59,
Visits: 373
carboncactus (21/06/2013)
benet (21/06/2013)
I would like to know however as i'm new to degassing is it normal for the resin to get worse before it gets better in the degassing process. I find that when i add heavily stirred ( big bubbles) resin to my chamber the big bubbles quickly go but are replaced by tiny ones that take a a further 10 minutes or so to finally rise and pop in my chamber. is this normal or do i have a leak or something causing a problem ?
How big is your vac chamber? I made a large one (about 10L) and it took way to long to evacuate. Eventually I made one just large enough for a cup of resin:
It evacuates in less than 30 seconds (tested with gauge)
If you get any bubbles after evacuating, what you're seeing is the solvent evaporating.
my chamber is pretty small, i use an asparagus steamer, it just holds a pint size plastic cup.
"Solvent evaporating" is that a problem ? When i degass, quite quickly the resin appears to "boil" a bit as the bubbles expand rise and pop but if i take the resin out of the chamber at that point its full with tiny bubbles that where not there when i started.. If this is solvent evaporating what should i do ?
Reply
Like
3
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
I guess it is technically "boiling", as youre lowering the air pressure, therefore lowering the boiling point. This happens somoetimes when you infuse with polyester.
When you degass, air will be evacuated fairly quickly. It's a 2 minute job, once you see the resin start to foam up and rise, stop. Let it settle, then evacuate a bit more. If it doesnt settle, air the chamber and youll see the resin flatten almost instantly. Pull some vacuum again, it should rise, but not so much. This is enough, if you start evacuating the styrene youll end up with a thicker resin, making the job harder for yourself.
Reply
Like
3
benet
benet
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 59,
Visits: 373
thanks carboncactus thats very useful, maybe the process is quicker than i thought. Im going to have to experiment some more.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Is it worthwhile degassing my coating resin in my vacuum chamber?
FiftyPence
-
12 Years Ago
Not really if you are going to apply it by brush then you will introduce air back into the resin...
wozza
-
12 Years Ago
As mentioned a heat gun works, but you have to be careful. too much heat and youll create a cluster...
carboncactus
-
12 Years Ago
acetone in a spray bottle. that sounds so dangerous.
benet
-
12 Years Ago
i have just been building a degassing chamber for this very purpose as i was finding tiny specks of...
benet
-
12 Years Ago
[quote][b]benet (21/06/2013)[/b][hr] I would like to know however as i'm new to degassing is it...
carboncactus
-
12 Years Ago
Carboncactus, Is that an connection for compressed air?
matthieutje65
-
12 Years Ago
It's just a standard male vacuum connection
carboncactus
-
12 Years Ago
[quote][b]carboncactus (21/06/2013)[/b][hr][quote][b]benet (21/06/2013)[/b][hr] I would like to know...
benet
-
12 Years Ago
I guess it is technically "boiling", as youre lowering the air pressure, therefore lowering the...
carboncactus
-
12 Years Ago
thanks carboncactus thats very useful, maybe the process is quicker than i thought. Im going to have...
benet
-
12 Years Ago
thanks for the feedback guys, in that case I will not bother degassing the resin as I will be...
FiftyPence
-
12 Years Ago
Do degass your resin,you are going to introduce some with your brush,but when you mix your resin...
Shaneer22
-
12 Years Ago
I degassed my new coating resin yesterday and it worked out perfectly even brushing it onto the part...
FiftyPence
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search