By FiftyPence - 6/20/2013 8:23:46 PM

Is it worthwhile degassing my coating resin in my easycomposites vacuum chamber before brushing it onto my part?

Thanks in advance for your advice.
By FiftyPence - 6/24/2013 9:56:06 AM

I degassed my new coating resin yesterday and it worked out perfectly even brushing it onto the part I had previously skinned in CF, thank you guys.