Look what happened to the gel coat :(


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Id say thats taken a whack.

Thicker the gelcoat, the more succeptable you are to cracks occuring with flex.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Jess8bit
Jess8bit
Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)
Group: Forum Members
Posts: 133, Visits: 566
Ok, I'll try to measure/estimate the thickness as soon I get the part back.
I think it is thicker than 0.2mm. Have to be softer with the spray gun I guess.

thank you Warren Smile
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Never had that with GC50 Hard to tell from the picture but the gelcoat does look pretty thick to me, especially around the corner area. You only need about 0.2mm. 

Regards Warren

Carbon Copies Ltd
Jess8bit
Jess8bit
Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)
Group: Forum Members
Posts: 133, Visits: 566
http://img442.imageshack.us/img442/6315/vgyz.jpg

Apparently this occured during the shipping but the package was ok and I suspect others reasons :

- Could it be due to the fact I left the gel coat (EC GC50) cure too long (more than 24hrs), causing delamination ?

- Or would it be because of the GC50 thickness (but does not seem too thick for me) ?

any other clue ?

feel bad right now Unsure 
frustrated cause the part was ok when I sent it.