With most composites ovens, by the time youve opened the doors, loaded the part in and shut it again, the temperature is probably 50 in the air anyway. Then it will take a good hour or so to soak through the part and mould and bring that upto temperature so realistically the pre-preg gets a fairly gradual temperature increase over the first few hours of the cure anyway.