Jess8bit
Jess8bit
Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)
Group: Forum Members
Posts: 133, Visits: 566
Hi guys,

Do you take any particular precaution when you trim your part with your Dremel ? How do you protect the surface from scratches that may occur during the trimming ?

I've had this problem : the srface was nice after demolding. After triiming the part, I've jad the bad surprise of observing many scratches and holes in the surface. My assumption is that I made the scratches myself simply by holding the part with my hand (with gloves on) and handling it durng the process (maybe because of carbone dust ?).

Hence the question. I'm thinking about covering the surface with a plastic film hold by masking tape all around the part edges.

What do you think ?

thank you !!
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Unless the part is really complicated with lots of recesses and steep sides etc you should not really need to stick the first layer down. Just pull vac in stages ie pull a small amount of vac and close off the valve, position the bag carbon etc and pull some more vac. Continue this way until you have full vac and everything is in place and tight against the mould surface. If you are not happy just release some of the vac and start the process again.

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Jess8bit - 12 Years Ago
NikCFC - 12 Years Ago
Jess8bit - 12 Years Ago
fgayford - 12 Years Ago
Jess8bit - 12 Years Ago
CarbonMike - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
matthieutje65 - 12 Years Ago
Jess8bit - 12 Years Ago
fgayford - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Shaneer22 - 12 Years Ago
Jess8bit - 12 Years Ago
Warren (Staff) - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search