Hi guys,

Do you take any particular precaution when you trim your part with your Dremel ? How do you protect the surface from scratches that may occur during the trimming ?

I've had this problem : the srface was nice after demolding. After triiming the part, I've jad the bad surprise of observing many scratches and holes in the surface. My assumption is that I made the scratches myself simply by holding the part with my hand (with gloves on) and handling it durng the process (maybe because of carbone dust ?).

Hence the question. I'm thinking about covering the surface with a plastic film hold by masking tape all around the part edges.

What do you think ?

thank you !!
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Ok 24 hours for the GC50 is ok but no longerWink
Ditch (stop using ) the spray tack. It is very easy to get a thick layer of it on edges and corners etc. When not using GC50 this is not really an issue as it will just effect the surface finish of the part which can be polished out but when using GC50 the spray tack forms a layer between the GC50 and the resin preventing a good bond between the two. Try the method I suggested before if you need to stick the carbon downWink

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Jess8bit - 12 Years Ago
NikCFC - 12 Years Ago
Jess8bit - 12 Years Ago
fgayford - 12 Years Ago
Jess8bit - 12 Years Ago
CarbonMike - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
matthieutje65 - 12 Years Ago
Jess8bit - 12 Years Ago
fgayford - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Shaneer22 - 12 Years Ago
Jess8bit - 12 Years Ago
Warren (Staff) - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search