Author
Message
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Are the joints butted together or overlapped?

Brian.
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi Brian, yes it's a butt joint.

Warren
            

Carbon Copies Ltd
Demlotcrew
Demlotcrew
Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)Supreme Being (151 reputation)
Group: Forum Members
Posts: 17, Visits: 140
FLD (14/03/2013)
Looks better than my first attempt.  Mines just wet lay though.  Its interesting to see peoples appraoch to this, I now stiffen the edge of the fabric by sticking a line of masking tape down the edge the acetoning off the tape.  It leaves some glue behind which stiffens up the weave allowing for easy positioning but also dissapears nicely.  This was my first go:



More info about how you acetone off the tape? 

Andrew
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
I think that is a good attempt...... It is easier with pre-preg though....