Right mandrel/mold for 90° bent carbon fiber tubes
Right mandrel/mold for 90° bent carbon fiber tubes
Post Reply
Like
8
Right mandrel/mold for 90° bent carbon fiber tubes
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
zeiss
zeiss
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 30
Hi all,
i'm buying some carbon fiber sleeves like the one in the image..
roughly 20 cm right + a 90° curve + another 20 cm right
with the diameter of 21 mm.
Upon your opinion what's the best and simple mandrel to create..
A copper tube rounded with pipe insulation foam...?
I read in some article that it could be the right solution..
I think only that it should not be so easy to take out
the copper tube once the carbon fiber is cured..
I imagine a different solution, the opposite of the previous one.
I would like to try to use a rubber hose of roughly 45 cm
( those used to water the garden). I do not know the technical term (I'm not native English speakers ..)
The outer diameter of the pipe must be equal to that which you want to obtain less the thickness of the sleeve of carbon fibers.
Then I would insert each of the two ends of the rubber tube two pieces of an adequate diametered rigid tube (aluminum stainless steel ...)
for a length of about 15 centimeters into the rubber hose...
Then I subdue the rubber tube by holding the ends of the two metal tubes and would insert it into a kind of template that keep it fixed and positioned so as to create the shape I wish. I_
once the carbon fiber is cured... i think that it could be more easy to take off the carbon fiber tube the mandrel..
First i could take off the metal pipe from the rubber hose..it should be easier than the first idea..
Tha pipe are straight... Then taking off the rubber hose from the carbon fiber tube created it should be not so difficult
because rubber i think it's more easy to go in the curves than copper.... :-)
What do you think about my idea...?
It might work ..? This will be my first attempt in the world of composites ..
Do you have any different ideas or suggestions..?
Thank you very much for taking the time in answering.
Attachments
Curved tubes.jpg
(
3.1K views,
98.00 KB
)
Tags
Carbon fiber
curved tube
mandrel
sleeve
tube
Reply
Like
8
Reply
zeiss
zeiss
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 8,
Visits: 30
Thank you very much Warren for your reply..!
I agree with your thought..
As you have some time please reply to my email about the diameter of this tubes
i've sent you last night..
As you can read i'm in doubt on what products to use for making 21mm diameter tubes..
If it's enough the
20mm diameter
or if it's better to go to the
40 mm type
..
As i read in a comment from another user (Chris) on the 20mm diameter carbon fiber braided sleeve,
i'd like also to be more sure about lenght and diameter to buy..
It's seem reading that post that he has some problem to make 21mm tubes with the 20 mm version..
and he have less lenght that expected at the 45° angle..
So as soon as i'll be sure on the right diameter and lenght to choose i'll order materials.
Thank you again for the help..
Zeiss.
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Right mandrel/mold for 90° bent carbon fiber tubes
zeiss
-
13 Years Ago
With a curved pipe like that, a flexible material in the middle is pretty much your only option as...
Warren (Staff)
-
13 Years Ago
Thank you very much Warren for your reply..! I agree with your thought.. As you have some time...
zeiss
-
13 Years Ago
For ease of use id go with the 40mm because its easier to contract braided sleeve than it is to...
Warren (Staff)
-
13 Years Ago
Ok.. Thank you Warren for your reply..It's clear.. 1) It's a little more difficult to work with...
zeiss
-
13 Years Ago
Hi, i find this silicone pipe that could be nice for use as a mold/mandrel (whit a metal tube...
zeiss
-
13 Years Ago
Theoretically those figures look about right. How close you get in practice could vary slightly....
Warren (Staff)
-
13 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search