What resins in Hi-Temp Skinning Kit?


Author
Message
ebf2k
ebf2k
Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)
Group: Forum Members
Posts: 9, Visits: 28
I want to order just the resins for doing some hi-temp skinning as found in the carbonmods kit
http://www.carbonmods.co.uk/Products/Carbon-Fibre-Skinning-Starter-Kit----High-Temp__CMCFSKHT300.aspx


I'm not sure which ones to order?  I can't find them based on the descriptions in the kit.

Also what is the difference between the base coat resin and the top coat?  Just the black pigmentation?

Thanks,
Eric
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K

Hi Eric,

 

These are the resins you need:

CarbonFibre High Temperature Laminating Epoxy Resin

CarbonSkinning Base-Coat - High Temp



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant