Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
repairs to an edge
repairs to an edge
Post Reply
Like
3
repairs to an edge
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
treeowen
treeowen
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 110
Hi,
In the photo is the shinpad area of a pair of tree climbing spikes. The left one is broken and to repair this do I need to create a mould?
I have watched all the other tutorials and have a fair idea of the process but none covered a damaged edge.
It doesn't have to be pretty and it is not being subjected to huge loads (I believe the damage occured in transit).
It is not PPE so there can be no liability issues.
If I have fun I may make some bits for my motorbike.
Any advice will be greatly received
Owen
Tags
edge repairs
Reply
Like
3
Reply
treeowen
treeowen
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 110
Fred,
Thanks, this does help a lot
Owen
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
repairs to an edge
treeowen
-
13 Years Ago
hello This is what I would do. Get a piece of aluminium sheet and bend it to follow the profile...
fgayford
-
13 Years Ago
Fred, Thanks, this does help a lot Owen
treeowen
-
13 Years Ago
Hi, Here is a view of my finished repair for anyone who is interested. Not much time was spent...
treeowen
-
13 Years Ago
nice job !
Jess8bit
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search