By treeowen - 4/5/2013 6:30:38 PM

Hi,
In the photo is the shinpad area of a pair of tree climbing spikes. The left one is broken and to repair this do I need to create a mould?
I have watched all the other tutorials and have a fair idea of the process but none covered a damaged edge.
It doesn't have to be pretty and it is not being subjected to huge loads (I believe the damage occured in transit).
It is not PPE so there can be no liability issues.
If I have fun I may make some bits for my motorbike.
Any advice will be greatly received
Owen
|
By Jess8bit - 6/3/2013 11:49:39 AM
nice job !
|
|