Hi,

In a recent thread there was a suggestion of making prototypes in Glass Fibre.
In doing this would I exchange carbon fibre 2/2 twill 3K 195g with woven glass 2/2 twill 200gsm or are there any differences which would make a another grade of glass more of a match? I will be using infusion.
I realise I will not get the strength of Carbon. It is just for me to practice before investing in Carbon fibre.

Brian.

Replies
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
hi brian,

i use woven glass to test as it behaves the same as CF under infusion situations,
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
I am looking for similar handling property's.
I am thinking more of practising technique. I am planning something a little complicated.
(For a beginner anyway!)

Brian.
Edited 12 Years Ago by Brian_s