Hi,
In a recent thread there was a suggestion of making prototypes in Glass Fibre. In doing this would I exchange carbon fibre 2/2 twill 3K 195g with woven glass 2/2 twill 200gsm or are there any differences which would make a another grade of glass more of a match? I will be using infusion. I realise I will not get the strength of Carbon. It is just for me to practice before investing in Carbon fibre.