advice/tips on repairing this BTCC!!


Author
Message
Phil
Phil
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 11, Visits: 54
hi all

bit of advice/ tips from the experts please Smile

basically picked up this bit of rare touring car history, its a 1999 Vauxhall Vectra BTCC touring car front splitter, as you can see its took abit of a beating in its time, this a little project for myself and to eventually fit it to my car for show perpose Smile





as you can see i have damage to this corner its cracked the carbon and actually took a chunk out of it and theres a hole, now im not after repairing it so that it can be used in racing terms.... but i would like to repair it so cosmetically it looks like new my plan was to fill the hole and smooth over the damage with fiberglass and then wetlay the whole splitter in carbon..... your thoughts please guys

many thanks

phil
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi, if you try and do a "patch repair" cosmetically it wont be great, ie you will see the patched area. If you want a cosmetically pleasing repair I would do as you suggest fill the hole/holes with GRP/Body Filler, finish and polish the whole front edge/ lip . Take a mould of the front lip. Then lay up a 3/4 layer "skin" from the mould and then bond that over the original.

Hope that makes sense, Warren

Carbon Copies Ltd