Group: Forum Members
Posts: 11,
Visits: 54
|
hi warren thanks for your help
i wasnt thinking a patch repair, i want the look to be almost flawless like its never been damaged, i intend to spray the whole splitter black so no repairs are visable threw the carbon and "skin" the whole lot, when you mention about making a mold for the front lip? why would you do this? i was hoping for wetlaying it straight onto the splitter in one and do a few layers, skinning it as a whole. (the white bit is actually paint thats been painted over carbon so underneeth that is pure carbon its one whole item not 2 seprate parts just incase you saw it as 2 parts) the blue top half is just a original bumper cut so it can be bonded onto the splitter and that bit will be painted the same colour as my car.
|