Hi all, newcommer here.  At the moment I am storing my resins ETC in my bedroom which I know is not ideal and would prefier to keep them in the workshop, the problem is that the workshop (insulated shed) can get very cold as I don't use it some weeks, I've seen the temp get as low as 3c in the cold spells we have been having and this can make resin etc go off.
I am considering making somekind of heated cabonet to store the resin in, perhaps a cupboard lined with 50mm Kingspan insulation.  Some form of small heating element and thermerstat to keep the tempreture of the cabonet above +15c to stop my expensive resins etc from perishing.  My fear is however is causing a fire, I know heat and flamable resins don't go togeather, especially if the thermerstat was to break and cause it to overheat.  so anyone have any tips on making a resin storage cabonet which will keep my resins at the correct storage temp and be safe?  Many thanks, lee.
Edited 12 Years Ago by Leew
Reply
alebassa
alebassa
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 48, Visits: 171
no, just standard bulb...

 

with two of these 100W each I can go to 70°C, of course if you need more temperature.. you need more power!


Alessandro
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search