Sure would like to see some pictures of intensifiers in action.

Anyone out there done this?

Thanks

Fred
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi Fred, I sometimes use pieces of sponge (from an old car seat) under the bagging film as intesifiers when doing Infusion. I will have a look and see if I have any pics.

Regards Warren

Carbon Copies Ltd