Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Intensifiers caul plates
Intensifiers caul plates
Post Reply
Like
3
Intensifiers caul plates
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
Sure would like to see some pictures of intensifiers in action.
Anyone out there done this?
Thanks
Fred
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Intensifiers caul plates
fgayford
-
12 Years Ago
Hi Fred, I sometimes use pieces of sponge (from an old car seat) under the bagging film as...
wozza
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search