ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 20
I am building a new glareshield for an airplane. The rear edge of the part has a bull nose and a slight return. All the angles are slightly open so parts un-mold without issue. But, getting fabric and resin to fill the corners in the underhang has proven difficult. I vacuum bag the part.
Does anyone have any tips for this sort of part? Thank you.
Tags
tips
underhang
Reply
Like
6
fgayford
fgayford
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
KingsleyHill (07/03/2013)
I am building a new glareshield for an airplane. The rear edge of the part has a bull nose and a slight return. All the angles are slightly open so parts un-mold without issue. But, getting fabric and resin to fill the corners in the underhang has proven difficult. I vacuum bag the part.
Does anyone have any tips for this sort of part? Thank you.
I am sure the members could help. There is not enough information to go on.
Supply some pictures of your plane and where the part goes? A sketch as well on what you are about to do would help.
Fred
Reply
Like
7
brasco
brasco
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
a video for a mold i posted showed filling possible sharp corners with fibers to reinforce the area. i have also read the uses for
chopped CF is to fill the odd voids and the resins can then encapsulate the fibers(chooped or loose strands). in the areas where cloth
doesnt want to co operate and stay in place.
i am unsure if my post if for your situation or not.
CarbonFiberCreations
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search