I had this random idea and wondered if anyone had tried it so thought I'd ask.  Feel free to tell me if I'm talking pish.

WRT envelope bags, has anyone tried one of those bag heat sealing tools to seal up the bag?  If they are good then it'd be dead easy (in my head anyway) slip the part in (ooer) and then just roll over each end and turn on the pump.  Interested to see if its been done.
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Never heard of WRT envelope bags, can you give a bit more information? Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




finallyaname
finallyaname
Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)
Group: Awaiting Activation
Posts: 6, Visits: 75
I'd guess WRT means With Relation To Wink
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Blush haha ok, not very familiar with english abbreviations Smile I was thinking it was some kind of brand/company

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
BigGrin

I've just engaged my brain and figured why it wont work.  Vac bac plastic is stable to heat (for ovening) so is unlikely to respond well to heat sealing!
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
FLD (05/03/2013)
, has anyone tried one of those bag heat sealing tools to seal up the bag?


This is one of the first things i thought when I saw a vac bag being done. I asked the question and was shot down immediately by the composites guru that was doing it. There will be loads of microscopic leaks apparently.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search