SteveRielly
SteveRielly
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 11
Hi All,
I've searching through here on keywords, and didn't see this question.
I'm looking to make carbon fibre body parts, using the blue carbon weave, where there is a direction of the weave based off the centre line of the car.
So looking from the front at say the bonnet, the right side has its weave head up to the right, and the left off to the left.
I've seen the odd thread on how to cut the weave to have a clean finish, so the next hard part is lining up the blue and black of the weave in the right directions,
something I'm thinking will take a fair bit of practice, and many many expletives.
My next area of concern, is keeping the two parts joined in the middle, and not moving while the infusion process is taking place.
Now I haven't seen this done first hand, only the YouTube vids, so unsure of the amount of vacuum pressure felt on the fabric, and if there is enough to actually
move it out of alignment, or even separate the two pieces.
The final product would have the blue carbon on the surface layer, 'normal' black carbon layers, maybe kevlar-carbon for additional strength.
Thoughts? Would this even be an issue, or should I use a tape of sorts down the centreline between the surface and 2nd layer to stop things from moving?
Reply
Like
3
Reply
SteveRielly
SteveRielly
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 11
I'm thinking then I'll have to ensure that I also line up the layers correctly, so that the blue is on top of the lower layer blue?
Didn't you notice 'discolouration' if much of the above layer black gets in there?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Keeping "joined' fabric in place during infusion
SteveRielly
-
12 Years Ago
Spray adhesive
Jack.Strong
-
12 Years Ago
If you are going to use spraytack make sure that it is compatible with the resin you are using or...
wozza
-
12 Years Ago
Thanks Wozza, very helpful info.....I didn't think at all about two layers of coloured due to...
SteveRielly
-
12 Years Ago
No problem. I have learnt the hard/expensive way :w00t: Attached is a pic of a part using 3 layers...
wozza
-
12 Years Ago
I'm thinking then I'll have to ensure that I also line up the layers correctly, so that the blue is...
SteveRielly
-
12 Years Ago
I am pretty sure that for something like a bonnet you should be ok as when the upper and lower skins...
wozza
-
12 Years Ago
planning on doing my body panels in much the same way... however I will use normal weave pro finish...
andygtt
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search