Hi Fred,I was at Banbury today with a friend using pre preg and this is not be all solution to a perfect finish,I personally get better results from infusion I found that you have to slow it down,my way is never use mesh to perimeter only in the part when resin hit peel ply its like hitting a wall,getting back to your question you want absolute vaccum,I know the easy composites use a resin rich surface layer to help with pin holes,but most off the structural parts I have seen are not cosmetically perfect.
|