Hi Scott No need for the inner tube just the vacuum bag. At least I hope so. I have my mold made and am about to attempt to do this with the EC prepreg I just received. Just like you saw on the video you posted. re: the manifold clip where he is seen pulling the vacuum bag through the inside. I will show step by step pictures if it works for me. Fred
|