The company I talked to had similar products, but they all react at temperatures higher then we need, I guess.




http://motoform.blogspot.se

Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
300degrees is indeed a very high temperature.
Nice to see we are a lot on here trying to find an answer! Cool

maybe look for another material? 
I was thinking of rubber, Sometimes when it gets really hot it expands, you have some rubber that they use for roads for example.
I remember that when I was little the rubber inbetween concrete plates expanded, you then get a sticky black gumball product.
the problem would be that it is not stiff enough while heated and wouldn't apply enough presure I think...

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




prsw
prsw
Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Here is scanned article about south African motorcycle carbon wheel manufacturer BST.
Images turn out small, see attached files below.
http://www.talkcomposites.com/Uploads/Images/277543b8-2c90-4b47-8889-e44f.jpg


http://motoform.blogspot.se

Attachments
BST100011304468900.jpg (562 views, 83.00 KB)
BST100021304468930.jpg (515 views, 113.00 KB)
BST100031304468953.jpg (556 views, 109.00 KB)
BST100041304468975.jpg (546 views, 108.00 KB)
BST100051304469000.jpg (556 views, 131.00 KB)
Edited 13 Years Ago by prsw
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
thanks prsw, 
interesting article, saved it on my computer Rolleyes

found this patent in meanwhile 
http://www.google.com/patents/EP1344634B1?cl=en&dq=expanding+silicone&hl=nl&sa=X&ei=tGQUUb7DBYKLhQfC1YHgBQ&ved=0CDcQ6AEwAQ
looks like the same technique but no specific brand of silicone to be found

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
just came up with a new theory,
what if you would work with some type of blatter filled with some air and water (like a balloon with some water in it), heat will make the water evaporate, causing presure inside the blatter and onto the part?!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




fgayford
fgayford
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hi Matt

I came across an article in (I think it was called) Composite World. There was an article with pictures of them makong a airfoil for a race car. They used silicone and a aluminium mould and heated press.It was very interesting and I would like to try it my self.

Fred
prsw
prsw
Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
yes maybe, but will the pressure be high enough?
The silicone gives a mechanical pressure, not like a "gas" pressure, but on the other hand thats what you get in an autoclave.

Crazy idea, use only water like in hydro forming.
Moulds have to be strong in any case.
Do you have a good system for making bladders?


https://www.youtube.com/watch?v=I_Z3AIFSd60


matthieutje65 (08/02/2013)
just came up with a new theory,
what if you would work with some type of blatter filled with some air and water (like a balloon with some water in it), heat will make the water evaporate, causing presure inside the blatter and onto the part?!



http://motoform.blogspot.se

Edited 13 Years Ago by prsw
prsw
prsw
Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)Supreme Being (908 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Update
I have called a company who told me to call another company who told me to call another company who told me to call the first company again.
I have not called them again yet, but will soon.

On of them was Wacker, http://www.wacker.com , they are quite specialized in silicones but they could not deliver this, at least the Swedish office
didnt know about a heat expanding silicone, but, they told me that it could in fact be an ordinary RTV2 silicone, that expands in heat just like any other material.


http://motoform.blogspot.se

Edited 13 Years Ago by prsw
fgayford
fgayford
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Here is the link to the article I spoke of. Its awesome and so high tech.

http://www.compositesworld.com/articles/high-speed-press-cure-for-high-speed-racers

Fred
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Thanks for the updates! Fred, they don't really talk about the silicone expanding but more as a core material that is removed afterwards?!
Prsw, thanks for the updates, maybe it would work with RTV silicone, but hard to find some data of it on the internet :s

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search