Polyester Infusion Resin?


Author
Message
Sharper
Sharper
Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)Forum Guru (54 reputation)
Group: Forum Members
Posts: 6, Visits: 35
I know the best stuff to use is epoxy infusion resin, but the price of polyester infusion resin is very tempting (almost half price).

Does anyone on here have much experience in using both types and offer any advice?

I have read tons of stuff about polyester resin giving off more fumes, shrinking when curing, and being better or worse at withstanding UV, but would like a real persons opinion, not just the science behind it all and people trying to up-sell their products.

Any advice or help would be greatly appreciated, as I am looking to by my resin infusion starter kit with pump next week. 

(||):::::::o: (||[[(())))))))))))))))))))))))))))))))))))))))))))))))))))))))))))))
Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
This was the finish I was getting out the mould using a polyester gel coat and then infusing the part