Peter at RLI Audio Lab
Peter at RLI Audio Lab
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 7
I need to cover the surface of a 'teardrop' shape (like a squashed tube with a sharp edge). Will the sleeve form well around the sharp edge or is it better to use sheets ? size is approx 300 m long by 100 m wide (and 300 mm long).
Reply
Like
3
neilb
neilb
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 107,
Visits: 504
thats pretty big! 300m x 100m
Reply
Like
3
fiberglasshawaii
fiberglasshawaii
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 6,
Visits: 7
That's huge! Hard edges are always tough to get super tight. It's always worked out better for us when you "soften" the edge of anything in order for a rigid material, like carbon, to be able to conform.
Fiberglass Hawaii Inc.
Oahu - Maui - Ventura
http://shop.fiberglasshawaii.com
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search