I need to cover the surface of a 'teardrop'  shape (like a squashed tube with a sharp edge). Will the sleeve form well around the sharp edge or is it better to use sheets ? size is approx 300 m long by 100 m wide (and 300 mm long).
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
thats pretty big! 300m x 100m
fiberglasshawaii
fiberglasshawaii
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 7
That's huge! Hard edges are always tough to get super tight. It's always worked out better for us when you "soften" the edge of anything in order for a rigid material, like carbon, to be able to conform.

Fiberglass Hawaii Inc.
Oahu - Maui - Ventura

http://shop.fiberglasshawaii.com
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search