Release now or be patient?
Release now or be patient?
Post Reply
Like
1
Release now or be patient?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
nutz
nutz
posted 11 Years Ago
ANSWER
Topic Details
Group: Forum Members
Posts: 14,
Visits: 58
Ok, so I laid up a fibreglass mold on Sunday and just seeing what peoples opinions are on when i should pop the mold, patience is starting to get the better with me as i want to get on with things.
Its been 3 days, should i leave it for another 4 days (i.e. 7 days) or will it be fine to pop now? Temperature in the shed has been a constant 8 degrees Celsius at the moment.
Tags
when to release mold
Reply
Like
1
Reply
Matthieu Libeert
Matthieu Libeert
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
In my opinion it's almost impossible for polyester to cure properly with those temperatures... polyester will need around 17°C to kick off
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Release now or be patient?
nutz
-
11 Years Ago
with PE, VE or epox resin? To my knowlegde, 7 days are with 20°C temperature, not 8°C.... You should...
_GABBER
-
11 Years Ago
Hi, its Polyester
nutz
-
11 Years Ago
[quote][b]nutz (30/01/2013)[/b][hr]Hi, its Polyester[/quote] Hi My experience with polyester is...
fgayford
-
11 Years Ago
In my opinion it's almost impossible for polyester to cure properly with those temperatures......
matthieutje65
-
11 Years Ago
Agree with Matt, your just stuck in the gel time
Jack.Strong
-
11 Years Ago
You should warm that up pronto. Bring it inside!!!
mikew
-
11 Years Ago
Post Reply
Like
1
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search