Ok, so I laid up a fibreglass mold on Sunday and just seeing what peoples opinions are on when i should pop the mold, patience is starting to get the better with me as i want to get on with things.
Its been 3 days, should i leave it for another 4 days (i.e. 7 days) or will it be fine to pop now? Temperature in the shed has been a constant 8 degrees Celsius at the moment.