Hi all

In the interest of increased rigidity in a panel........


Ive been producing skateboards using a 10mm wooden core with 600 weight plain weave glass fiber skins top and bottom. They work pretty well.

However i have seen boards using a carbon skin on the underside which is done with the intention of increasing stiffness.

I was wondering about this and thought that, given in my case the core is skinned top and bottom and that grp is generally stronger in elongation than compression i would be better of if i skinned the upper side of the board in 450 carbon and the underside still with 600 grp.

My thinking is that i would have a better balance in the strength of the skins ( the upper being stronger to withstand compression the lower being slightly weaker but effectively strong in elongation) and hence a stiffer board than if i just skinned the bottom in carbon and left the top in grp...?

Im wondering if the use of carbon on the underside of a skateboard is more about aesthetics  (as its on show, the top normally covered in grip tape) and less about engineering.

Any experienced advice much appreciated.

Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
have you thought about using FG or Carbon fiber inbetween the layers of wood? before pressing the board together?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search