You need a bigger cup. Some resins and especially silicones can froth up to several times their original volume, so you need a bigger cup to ensure it does not overflow.
In some resin casting applications there are vacuum casting machines for pouring under vacuum but that is not applicable to laminating resins.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|