400 twill v 200 twill strength


Author
Message
chriscnf
c
Supreme Being (500 reputation)Supreme Being (500 reputation)Supreme Being (500 reputation)Supreme Being (500 reputation)Supreme Being (500 reputation)Supreme Being (500 reputation)Supreme Being (500 reputation)Supreme Being (500 reputation)Supreme Being (500 reputation)
Group: Forum Members
Posts: 34, Visits: 2.7K
Hi guys...Ill get some into try now that its easily available, but do you find that 400 twill is twice as strong as two 200 twill layers. I'm hoping its just as drapeable and the weave is more stable than the 200 twills.
Cheers...Chris