Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
I would increase the amount of spiral around the resin feed to make a nice U shape going at least half way across the mould. You don't normally need spiral on the vacuum side as long as the vacuum port is on the edge of the cloth and peel ply. As per the video you could even make a resin break.