Hi everyone. this might be a bit of a longshot but im just wondering, which manufacturer boasts the highest temperature resistance for their resin when cured. thanks
Reply
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
cole-P - 9/4/2021 8:38:19 PM
Hi everyone. this might be a bit of a longshot but im just wondering, which manufacturer boasts the highest temperature resistance for their resin when cured. thanks


Araldite® LY 8615 Resin with hardener Aradur® 8615 has a Tg of 217°C.