Best release wax to avoid fish eye


Author
Message
carbon man
carbon man
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Hi, what is the best release wax available in the UK. Or even worldwide, if its good il buy it!

Im looking for a wax good enough to release infusion parts from uni mould and also good enough that the brush in clear gel coat doesn't fish eye and pool.

Thanks
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You're fighting a losing battle, brushing clear gelcoats just isn't a very viable option. It's a compromise, and the downsides of that compromise are sags, pooling and fish-eyeing. 

I can understand not having spray equipment for a hobby, but I would suggest checking out a Preval sprayer. Cheap and easy to use and will spray Glosscoat fine. This way you can spray on a 'dust' coat, allow it to cure to a tack, then spray another coat to full thickness without fisheyes.
carbon man
carbon man
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Hanaldo - 6/23/2021 8:47:49 AM
You're fighting a losing battle, brushing clear gelcoats just isn't a very viable option. It's a compromise, and the downsides of that compromise are sags, pooling and fish-eyeing. 

I can understand not having spray equipment for a hobby, but I would suggest checking out a Preval sprayer. Cheap and easy to use and will spray Glosscoat fine. This way you can spray on a 'dust' coat, allow it to cure to a tack, then spray another coat to full thickness without fisheyes.

OK cool. I do have spray gun set up I use to spray 2k clear coat. Would this gun work?

But I have just bought the preval never seem then before! But looks quick and easy. I guess you just clean out the same as a spray gun

Also what is the maximum time i could leave gloss coat in mould before the infusion?

Edited 5 Years Ago by carbon man