Certainly I would Agree, go for a proper structural adhesive every time for bonding applications like this as the bond strength, especially for relatively small bonding surface areas, is much stronger.
If you were just bonding two large sheets together with only light structural expectations, then yes a resin over such a large surface area is probably strong enough. But for smaller areas, a dedicated structural adhesive will out perform a laminating resin.