Dear Friends,

I am going  to start my own project - Building a Hi-Tech furniture for kitchens. The tentative project commencement period - Middle of January 2013. Honestly, I am familiar with composites works as I have extensive experience in aeromodelling. Sure, some techniques were acquired from e-periodicals and video tutorials like those presented by Matt - Carbon Bonnet series.

The idea is to create the furniture which will be compliant to the following specifications:

1. Ultra-light and strong, tenacity to shocks

2. Perfect, radiant surface and durability,

3. Amature friendly (easy to assemble and disassembling properties),

4. High UV and heat resistance,

5. Uniqie in-built user freiendly design. 

Anyway, dear EC members, I would appeal for some hints and practical advises for my project. So let me start my narration. Please correct me if I am wrong.

The panels shall be of both right geometrical dimensions and curvilinear. For this project I am going to use combination of 3 colours (i) horizontal panels of black colour (carbon), (ii) vertical panels and interiors (red, dyed epoxy gelcoating, filler - glass fibre), (iii) foot panels - Alufibre carbon. The sample shall be like the furniture presented in attechment hereto.      

Question 1: What is the most optimal thickness of panels? I think 1 mm for doors is sufficient. Whereas other vertical panels (bearing pulleys) might be of 3 mm. The horizontal panels shall be 4 mm on top and 5-6 mm at edges/rims. Is my judgement fair or it is a waste of materials and money?

Question 2: What materials do I have to use as fillers for panels? Plyurethane blocks for plain surfaces and aramid honeycombs for curvular laminates? I need optimal advise. The panel should be cost efficient and possess good mechanical resistance properties.

Question 3: What is the best way to bond prefabricated composite laminate to filler materials and cover panel to get strongly fit sandwich with perfectly finished edges and corners? I need the glues and adhesives best pertinent to my demands.

Question 4: What glues can I best use to bond prefabricated panel to aramid/aluminum honeycombs? 

Please advise all the materials which may help me get best and cost efficient result.

Thanks in advance,

Communicator

All Well that End Well.

Communicator
Attachments
fd2_517_clip_image001.jpg (348 views, 61.00 KB)
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
trying to help--EC has adhesives to join cf, and there are many other adhesives that can as well. the 3m scotchweld series work very well.


CarbonFiberCreations



brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
and you have a very AWESOME idea !!


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search