Hi, so I have this mould that will be used just one time and theb scrapped.
It is made with epoxy gelcoat and a few layers of 200gsm cloth laminated with epoxy.
I want to infuse the part and I think the mould is too flexible for the job.
What do you suggest as the cheapest way to stiffen it?
I was thinking about breather cloth impregnated with cheap polyester resin but maybe you have better and cheaper ideas?

Thanks for any advice!
Attachments
signal-2020-12-22-180817.jpg (230 views, 480.00 KB)
Reply
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Warren (Staff) - 12/23/2020 3:51:44 PM
As oakmont says, eps or some foam or even wood strips used as stiffening ribs.  Couple of layers of glass over and it should help considerably. 

Thank you both for your suggestions!
Would polyester damage in any way the epoxy?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
oekmont - 5 Years Ago
Warren (Staff) - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
raygun - 5 Years Ago
Hanaldo - 5 Years Ago
raygun - 5 Years Ago
Hanaldo - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search