Hi, so I have this mould that will be used just one time and theb scrapped.
It is made with epoxy gelcoat and a few layers of 200gsm cloth laminated with epoxy.
I want to infuse the part and I think the mould is too flexible for the job.
What do you suggest as the cheapest way to stiffen it?
I was thinking about breather cloth impregnated with cheap polyester resin but maybe you have better and cheaper ideas?

Thanks for any advice!
Attachments
signal-2020-12-22-180817.jpg (334 views, 480.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 6 Years Ago
oekmont - 6 Years Ago
Warren (Staff) - 6 Years Ago
mporta71 - 6 Years Ago
Hanaldo - 6 Years Ago
mporta71 - 6 Years Ago
raygun - 6 Years Ago
Hanaldo - 6 Years Ago
raygun - 6 Years Ago
Hanaldo - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search