Hello
I have made some molds of CS25 Condensation Cure Silicone Rubber

but since the parts I make in the molds are for cars, you want to be able to paint them in a safe way, this becomes very difficult as the parts become very contaminated with silicone from the moulds 

so my question is if it is possible to make the molds of px60 instead of getting away from the silicone?
if so, what should I use for release agents?
or is it possible to completely remove the silicone from the products made in the molds?

best regards Johan

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Generally in silicone moulds, by the time you have sanded the cast resin ready for painting and wiped down with IPA/acetone, there is no problem with paint adhesion. Quite a lot of crafters use silicone moulds for resin casting work where the parts are subsequently painted.

If you did want to go down the PX 60 route, you would probably need a spray on release agent for ease of use.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search