Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
It isn't that the pleat in the bag causes any bridging, more that if you have a large pleat in the bag then this is film that isn't in contact with your mould - so you should try to spread those large pleats across to make several smaller pleats, which means you have more bagging film in contact with the mould in that area.
Definitely getting there! I think a bit more time positioning the bagging stack and you will eliminate the bridging entirely.
|